Bectron® PK 4340
thick-film conformal coating, ELANTAS Europe
| Chemical base | One-component polyurethane duroplastic (encapsulated polyisocyanate), thixotropic |
|---|---|
| Colour | black |
| Viscosity | 8,000–11,000 mPa·s (23 °C, DIN 53019, D = 15 s⁻¹) |
| Density | 1.26–1.30 g/cm³ (20 °C, ISO 2811-2) |
| Cure | 90 °C: 30 min (TDS range 25–35 min), recommended by ELANTAS; 80 °C: 60 min (60–70) |
| Cure temperature | 90 °C |
| Hardness | 60–80 Shore A (23 °C, ISO 868) |
| Dielectric strength | 20–24 kV/mm (23 °C, IEC 60455-2) |
| Thermal conductivity | 0.22–0.28 W/m·K (23 °C, DIN 52616) |
| Glass transition temperature | -45 to -50 °C (IEC 61006) |
| Operating temperature | -60 to +125 °C (temperature cycling) |
| Water absorption | 0.9–1.2 % (24 h, 23 °C, DIN EN ISO 62) |
| Shelf life | 6 months at -10 to +25 °C |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)TDS N° 1893 Rev. 2, 03/2024 · 3 pages, 138 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298