VFP CEL001
Carbon Electron 001, VFP Ink Technologies
| Printing | Screen, 79–120 threads/cm; prints over SE, SETF, FSE |
|---|---|
| Cure | 120–150 °C / 3–5 min |
| Resistivity / insulation | ≤ 120 Ω/sq/mil at 120 °C / 5 min |
| Substrates | Paper, cardboard, PET, treated polyester |
| Shelf life (closed pot, +5…+35 °C) | 1 year |
| Documented with | Over SE, SETF, FSE |
Source: the VFP Ink Technologies datasheet (TDS) of each grade; NIR drying and anilox values from VFP’s presentation of April 2026. Values are VFP’s; VFP advises a preliminary test on your substrate.
ELANTAS discontinued its Bectron® printed-electronics inks in September 2026; we help you qualify the VFP equivalent on your screen and substrate.
Expected track resistance
From the sheet resistance in the TDS (≤ 120 Ω/sq/mil at 120 °C / 5 min) and your track geometry.
Calculated resistance
Do not dilute the ink: dilution “would deteriorate the conductive properties” (VFP TDS).
Our calculation: R = value per mil × (length ÷ width) × (25.4 µm ÷ dry thickness). Default: the geometry VFP uses for the SE TDS figure (6 cm × 1 mm × 8 µm). On your press, resistance depends on the substrate, the dryer profile and the real deposit thickness.
VFP CEL001
- Samples
- 100–500 g
- Minimum order
- 1 kg per silver ink; 500 g per dielectric; other grades on request
- Lead time
- 5–15 business days from order
Other inks
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298