VFP ECV004

Dielectric Varnish-004, VFP Ink Technologies

Tab. 1Process data according to VFP
PrintingScreen, 79 or 90 threads/cm
CureBroad-spectrum UV (mercury/xenon), > 300 mJ/cm²; peaks 359/365/380/383 nm
Resistivity / insulationInsulation > 2 TΩ; breakdown 4,000 V for 2 layers
SubstratesPaper, PET, PC, treated polyester
Shelf life (closed pot, +5⁠…⁠+35 °C)1 year
Documented withSilver Electron range

Source: the VFP Ink Technologies datasheet (TDS) of each grade; NIR drying and anilox values from VFP’s presentation of April 2026. Values are VFP’s; VFP advises a preliminary test on your substrate.

ELANTAS discontinued its Bectron® printed-electronics inks in September 2026; we help you qualify the VFP equivalent on your screen and substrate.

VFP ECV004

VFP ECV004 Dielectric Varnish-004 Request a sample or TDS
Samples
100–500 g
Minimum order
1 kg per silver ink; 500 g per dielectric; other grades on request
Lead time
5–15 business days from order

Other inks

Silver inks

SE · SETF · SELEC · LV-SELEC · SES · FSE · SECTR-I01

Carbon inks

CEL001 · CEL003

Dielectric varnishes

ECV003

Piezoelectric inks

PEUV · PESOL

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298