VFP CEL003

Carbon Electron 003, VFP Ink Technologies

Tab. 1Process data according to VFP
PrintingScreen, 79–120 threads/cm; prints over SELEC, LV-SELEC
Cure120–150 °C / 3–5 min; NIR 2 s
Resistivity / insulation120 Ω/sq/mil at 120 °C / 5 min
SubstratesPaper, cardboard, PET, treated polyester
Shelf life (closed pot, +5⁠…⁠+35 °C)1 year
Documented withOver SELEC, LV-SELEC

Source: the VFP Ink Technologies datasheet (TDS) of each grade; NIR drying and anilox values from VFP’s presentation of April 2026. Values are VFP’s; VFP advises a preliminary test on your substrate.

ELANTAS discontinued its Bectron® printed-electronics inks in September 2026; we help you qualify the VFP equivalent on your screen and substrate.

Expected track resistance

From the sheet resistance in the TDS (120 Ω/sq/mil at 120 °C / 5 min) and your track geometry.

Calculated resistance

Do not dilute the ink: dilution “would deteriorate the conductive properties” (VFP TDS).

Our calculation: R = value per mil × (length ÷ width) × (25.4 µm ÷ dry thickness). Default: the geometry VFP uses for the SE TDS figure (6 cm × 1 mm × 8 µm). On your press, resistance depends on the substrate, the dryer profile and the real deposit thickness.

VFP CEL003

VFP CEL003 Carbon Electron 003 Request a sample or TDS
Samples
100–500 g
Minimum order
1 kg per silver ink; 500 g per dielectric; other grades on request
Lead time
5–15 business days from order

Other inks

Silver inks

SE · SETF · SELEC · LV-SELEC · SES · FSE · SECTR-I01

Carbon inks

CEL001

Dielectric varnishes

ECV003 · ECV004

Piezoelectric inks

PEUV · PESOL

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298