VFP ECV003
Dielectric Varnish-003, VFP Ink Technologies
| Printing | Screen, 79 or 90 threads/cm |
|---|---|
| Cure | Broad-spectrum UV (mercury/xenon), > 300 mJ/cm²; peaks 359/365/380/383 nm |
| Resistivity / insulation | Insulation > 2 TΩ; breakdown 4,000 V for 2 layers |
| Substrates | Paper, PET, PC, treated polyester |
| Shelf life (closed pot, +5…+35 °C) | 1 year |
| Documented with | Silver Electron range |
Source: the VFP Ink Technologies datasheet (TDS) of each grade; NIR drying and anilox values from VFP’s presentation of April 2026. Values are VFP’s; VFP advises a preliminary test on your substrate.
ELANTAS discontinued its Bectron® printed-electronics inks in September 2026; we help you qualify the VFP equivalent on your screen and substrate.
VFP ECV003
- Samples
- 100–500 g
- Minimum order
- 1 kg per silver ink; 500 g per dielectric; other grades on request
- Lead time
- 5–15 business days from order
- UV dose
- Calculate it for your lamp
Other inks
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298