Which application method suits each Bectron® material
This note is application know-how: which application method suits which material, so the coating, the potting and the cure work together on your line.
| Application | Bectron® materials | Application method |
|---|---|---|
| Conformal coating | ||
| Thin film, selective | PL 4122-40, PL 1102, PT 4700 N, PL 4122 range | Selective spray or film-coating valve on a coating robot |
| Thick film, selective | PT 4600, PT 4601, PK 4340 | Bead or film dispensing; PT 4600 cures under UV, shadow areas by moisture |
| Melting resins | MR 3402, MR 3405, MR 3406 | Heated hot-melt application at the temperature the TDS gives |
| Potting and encapsulation | ||
| 2-component polyurethane | PU 4501, PU 4522 | Meter-mix-dispense with static mixer, at the TDS mix ratio |
| 2-component silicone gel | SG 75V1-15, SG 75V1-60, SG 75V1-75 | Meter-mix-dispense; low viscosity flows into gaps |
| 2-component epoxy | EP 5502, EP 5504 | Meter-mix-dispense with static mixer |
| 1-component heat-curing polyurethane | PK 4344 | Volumetric 1-component dispensing, then oven cure |
| Dam and fill | ||
| Dam | PT 4606 | High-viscosity volumetric bead around the area |
| Fill | PK 4342, PT 4600 | Lower-viscosity fill inside the dam |
UV-curing materials need a matching lamp and dose. See the worked example.
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298