Technical guides

Each guide starts from a problem on the line and answers it with datasheet values, with the source next to every number.

31 October 2026

Bectron® printed-electronics inks discontinued: VFP silver, carbon and dielectric alternatives

ELANTAS ended the Bectron printed-electronics ink line in Sep 2026. VFP silver, carbon and dielectric inks: cure, mesh and resistivity from VFP data.

Printed electronics

18 October 2026

Conformal coating vs potting for power electronics: what the datasheets show

In Bectron TDSs the thick-film coating PK 4340 lists 0.22–0.28 W/m·K; the potting compounds PU 4527, SK 75V2-45 and PU 4526 list 0.54 to 0.70 W/m·K.

Conformal coating · Potting and encapsulation · Thermal management

PU 4526 · PU 4515 · PU 4527 · SK 75V2-45 · PK 4340 · PK 4342 · PT 4600 · PL 4122-40 · MR 3406

18 October 2026

Hot-melt (melting resin) PCB coating: what application temperature?

The ELANTAS TDS for Bectron MR 3406 asks for 190–200 °C at the nozzle and a reservoir at 170 °C for 1 day maximum; 180 °C is the viscosity reference.

Melting resins (hot melt)

MR 3406 · MR 3406 FR · MR 3404

18 October 2026

How to protect a PCB from condensation: coating options with datasheet values

Condensation needs a coating that stays insulating when wet. Bectron TDS values after water immersion: PL 4122-40 E, PT 4600, PK 4340, MR 3406.

Conformal coating

PL 4122-40 · PT 4600 · PK 4340 · MR 3406

18 October 2026

Silicone vs polyurethane potting: temperature, cure and moisture from the TDS

Bectron SK 75V2-45 silicone potting is rated −55 to +200 °C; the polyurethanes PU 4515 and PU 4526 stop at +150 °C and +130 °C (ELANTAS TDS).

Potting and encapsulation

SK 75V2-45 · SK 75V2-65 · PU 4515 · PU 4526 · PU 4527

18 October 2026

Thin-film vs thick-film conformal coating: solvent, cure and film build compared

PL 4122-40 E thin film: 40 % solids, about 80 mPa·s, 16 h cure at 23 °C. PT 4600 thick film: solvent-free, 200 ± 50 µm, UV-cured in about 5 s (TDS).

Conformal coating

PL 4122-40 · PL 4122-45 · PT 4600 · PK 4340 · MR 3406 · AC 93 · 217 · 239 · 300

18 October 2026

Why a UV-cured conformal coating stays tacky

Tacky UV coating usually means too little UVA dose or shadow areas still moisture-curing. PT 4600 TDS: 2,500–3,500 mJ/cm² UVA, 2–3 days shadow cure.

Conformal coating · UV curing

PT 4600 · PT 4601

18 October 2026

How to calculate UV dose on a conveyor: mW/cm², mJ/cm² and belt speed

Dose (mJ/cm²) = irradiance (mW/cm²) × exposure time (s); time = lit length ÷ belt speed. Worked example for a 3000 mJ/cm² UV coating.

UV curing

PT 4600 · PT 4601

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice